JP6563099B1
To provide a method for cutting a steel fiber reinforced concrete provided on a steel plate, which can appropriately cut the steel fiber reinforced concrete without damaging the steel plate. The steel fiber reinforced concrete 6 installe...  
JP6554242B2
[Problem] To provide an adsorbent, a contaminated water treatment body, and a landfill treatment site/paved road using the adsorbent, the adsorbent having a simple and effective structure that uses fine particulate clay minerals and exhi...  
JP6542015B2  
JP6541238B2  
JP6535193B2
To provide an injection material for semiflexible paving having excellent freeze-thaw resistance as well as excellent in development of initial strength and a semiflexible paving using the injection material.There are provided an injecti...  
JP6535636B2  
JP6534291B2  
JP6535639B2  
JP2019094646A
To provide an antislip coating material coating device capable of uniformly coating an antislip coating material in a state of mixing an aggregate and a binder at a prescribed rate.An antislip coating material coating device comprises a ...  
JP6532163B2  
JP6531022B2  
JP6530842B1
To color a cement-based base material in a cement-based decorative material while maintaining the appearance of the decorative member in the decorative surface by applying the cement-based base material and the decorative member to an ex...  
JP2019085860A
To provide a construction method for cast-in-place water retentive pavement which can be installed in a short time with less labor.A construction method for a cast-in-place water retentive pavement, comprises the steps of: coating concre...  
JP2019082022A
To provide an asphalt mixture which suppress void blocking or flow to keep excellent noise reduction and draining properties with excellent durability.An asphalt mixture made of a mixture of an aggregate, asphalt, and an asphalt additive...  
JP6511680B2  
JP6511618B2  
JP6504949B2  
JP6499802B1
To provide a steel deck pavement structure capable of surely preventing peeling of a fiber reinforced concrete pavement such as SFRC pavement and preventing deterioration of a steel deck. In a steel deck pavement structure in which a fib...  
JP2019052523A
To provide a concrete pavement and the like having a large bending strength at a long-term material age, a small fatigue degree, and a long service life even in a region where the annual mean air temperature is high.A concrete pavement o...  
JP6479448B2  
JP6477390B2  
JP6479559B2  
JP6474085B2
The present application discloses compositions and methods for improving or enhancing the paving or re-paving of asphalt to road surfaces comprising the addition of the composition to the asphalt.  
JP6475390B1
To provide a technique for improving water resistance performance by suppressing peeling of asphalt. The asphalt composition of the present disclosure contains at least an asphalt base oil and a silane-containing coupling agent, and the ...  
JP2019019544A
To provide a pavement and pavement construction method capable of easily filling a cement milk cavity.A pavement 1 comprises a support base 10 and a semi-flexible pavement 20 formed on the support base 10. The semi-flexible pavement 20 c...  
JP6467087B1
To provide an asphalt mixture for thin-layer pavement which can be supplied in large quantities at low cost and can improve durability, a method for repairing a paved road using the mixture, and a paved road repaired by the mixture. To d...  
JP6463531B2  
JP6465762B2  
JP2019502007A
The present invention is an asphalt regenerant comprising a specific styrene-based block copolymer, a bio-based oil or a bio-based oil blend, and an antioxidant system. The bio-based oil or bio-based oil blend has a flash point above 230...  
JP6458197B1
To provide a method for repairing a structure in which the filling property against cracks is good and the repair can be easily performed, and the aesthetic appearance and durability of the repaired portion are improved at low cost. A wa...  
JP6457842B2  
JP6456417B2
Provided are: a liquid-addition solidifying composition that solidifies due to the addition of liquid and can be disposed of in a similar manner to soil after solidifying; and a solidified body in which the liquid-adding solidifying comp...  
JP6458194B1
To provide a normal temperature asphalt mixture capable of improving durability after pavement and workability at the time of pavement in a low temperature environment lower than normal temperature. The room temperature asphalt mixture a...  
JP2019007176A
To provide a radical-polymerizable resin composition which has fast curability that cures in a short time after construction, has no smell, does not create cracks on a coated surface, and makes good finish even if applied to a pavement w...  
JP6447003B2  
JP6448031B2  
JP2018538683A
The present invention is for inductively supplying energy to an electric or hybrid vehicle, the electric power is non-contactly guided to a secondary coil provided in the vehicle supplied from a primary coil coupled to the road. Is trans...  
JP6439025B2
Described are materials (14) and structures (10) for absorbing energy. The materials (14) and structures (10) are well suited for arresting aircraft and other vehicles, although their purposes need not be so limited. Also detailed are pa...  
JP2018193762A
To provide a gas delivery discharge system in a pavement body which stably demonstrates an insect repelling effect and a fragrance effect by supplying a gas having an insect repelling function and an aromatic function in the pavement bod...  
JP6434925B2
The present invention relates to a paving method of forming an intermediate layer, where a non-solidifying rubberized asphalt penetrates, on an asphalt mixture for base layer or a cement concrete to provide a permeable layer and an imper...  
JP6434917B2
Methods for reducing asphalt pavement thickness are provided. A method for producing thin asphalt pavement includes combining a base asphalt, an oxidized polyolefin, and an aggregate to form an asphalt paving material. A layer of the asp...  
JP2018188890A
To provide a paving machine capable of constructing a paving body having water barrier properties in a lower area of pavement of a single pavement layer and using a porous concrete having water permeability and noise reduction performanc...  
JP6430734B2  
JP2018178602A
To provide a technology for reducing a period of nonslip pavement construction on site.A transportable nonslip pavement material (10) is made of a mixture containing at least hard aggregate and a binder formed in a thin plate fashion, an...  
JP3218708U
To provide a water-retaining block pavement capable of mechanically supplying water when the temperature of the pavement rises without using an electric circuit. A plurality of water-retaining blocks 10 arranged in parallel on a base lay...  
JP6416012B2  
JP6417100B2  
JP6408301B2  
JP6406090B2  
JP6408193B1
It is a method of forming a stone slab-like pavement such as stone pavement with natural stone on an existing or new pavement surface, in which the pavement process of paving the pavement body (2) and the pavement surface (1) of the pave...  