To produce a special polymer having a high-molecular weight or a high degree of branching in a highly efficient manner without deteriorating the same, by uniformly plasticizing and melting the special polymer having a high-molecular weight or a high degree of branching by a pair of kneading screws even if the number of rotations of the kneading screws is low.
A material to be kneaded having a high-molecular weight or a high degree of branching and easily deteriorative is stepwise supplied into a pair of left and right kneading chambers formed in a barrel 3 in a mutually communicating state and kneaded and melted in a plurality of kneading zones 15 and 16 formed to a pair of left and right kneading screws in an axially separated state over two stages while fed to the downstream side by a pair of the left and right kneading screws inserted into the respective kneading chambers in a freely rotatable manner.
COPYRIGHT: (C)2003,JPO
Hiroyuki Shibata
Kimio Inoue
Chisso Petrochemical Co., Ltd.
KABUSHIKI KAISHA KOBE SEIKO SHO
JP6182756A | ||||
JP2000246732A | ||||
JP3176932B2 | ||||
JP7045551B2 | ||||
JP5008221A | ||||
JP2001205625A | ||||
JP8099313A | ||||
JP8174638A |