Abstract:

To provide a method for producing nickel oxide which can obtain nickel oxide in which an alkali metal content is ≤100 ppm with respect to a transition metal(s) (including Ni) incorporated therein without producing poisonous gas.

The method for producing nickel oxide includes: a heating stage where a nickel hydroxide-containing precursor in which one or more kinds of first period transition metals other than nickel are comprised, and also, an alkali metal(s) used for neutralizing treatment is left is used as raw material, and the precursor is heat-treated at 300 to 1,000°C, so as to produce nickel oxide in which the average pore size of the grains is ≥25 Å, also the pore volume in the grains is 0.001 to 0.20 cm3/g, and further, the crystal system essentially consists of Fm3m; and a water-washing stage where the nickel oxide obtained in the heating stage is water-washed.

COPYRIGHT: (C)2009,JPO&INPIT


Inventors:
Dozen Kyosuke
Shibuya Eika
Yoshiaki Nitta
Application Number:
JP2007315828A
Publication Date:
December 14, 2011
Filing Date:
December 06, 2007
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Tanaka Chemical Research Institute Co., Ltd.
International Classes:
C01G53/00; H01M4/52; H01M4/86
Domestic Patent References:
JP7010544A
JP11054159A
JP6096768A
JP11079752A
Attorney, Agent or Firm:
Hiroshi Yamazaki
Mitsuo Tanaka
Yasushi Ohata



 
Previous Patent: JPS4837650

Next Patent: JPS4837652