To provide a heat shrinkable multilayer film which has high light shielding property, holds quality of content, has an appropriate mechanical property, and a high heat shrinkable property, and also to provide a heat shrinkable label setting the heat shrinkable multilayer film to be a base film.
In the heat shrinkable multilayer film, a front and rear layer containing a styrene-butadiene copolymer is laminated through a core layer containing the styrene-butadiene copolymer and titanium dioxide. The styrene-butadiene copolymer composing the front and rear layer contains a styrene component of 75-90 wt.% and a butadiene component of 10-25 wt.%, and Vicat softening temperature is 80-90°C. The styrene-butadiene copolymer composing the core layer contains a styrene component of 70-80 wt.%, and a butadiene component of 20-30 wt.%, while the Vicat softening temperature is 70-80°C, and also contains titanium dioxide of 8-40 wt.% for the gross weight of the heat shrinkable multilayer film.
COPYRIGHT: (C)2009,JPO&INPIT
Kiyasu Ishikawa
JP9272182A | ||||
JP2003236930A | ||||
JP2005239799A | ||||
JP2005263938A | ||||
JP2002278460A | ||||
JP2006212785A | ||||
JP2000229357A |
WO1999029490A1 |
Yasuo Yasutomi
Katsutoshi Moroda
Takao Okamoto