Abstract:

To provide a modified styrene-fumaric acid copolymer reusable for a low shrinkage material of a thermoplastic resin.

The modified styrene-fumaric acid copolymer is prepared by subjecting the fumaric acid structure portion of a styrene-fumaric acid copolymer to a condensation reaction. The condensation reaction is conducted by the reaction with acetic anhydride or by the thermal dehydration reaction. The styrene-fumaric acid copolymer is prepared by decomposing a thermosetting resin containing a polyester and its crosslinked portion with supercritical water. Preferably, the decomposition is conducted in the presence of an alkali.

COPYRIGHT: (C)2008,JPO&INPIT


Inventors:
Toyoyuki Urabe
Yoshimura Tsuyoshi
Application Number:
JP2007016625A
Publication Date:
August 15, 2012
Filing Date:
January 26, 2007
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Panasonic Corporation
International Classes:
C08F8/48; C08F212/08; C08F283/01; C08J11/14
Domestic Patent References:
JP2000281848A
JP2005336322A
JP63097601A
JP62127302A
JP56036504A
JP9176411A
JP7150024A
JP2006036938A
Foreign References:
WO2006057250A1
Attorney, Agent or Firm:
Toshio Nishizawa