Title:
酸化物超電導素線の集合化導体、及びこの集合化導体の製造方法
Document Type and Number:
Japanese Patent JP5118412
Kind Code:
B2
Abstract:

To provide an assembled conductor of a plurality of oxide superconducting element wires which reduces biased current flow occurrence while using a plurality of oxide superconducting material wires, and to provide a manufacturing method of such an assembled conductor of oxide superconducting element wires.

The assembled conductor includes the oxide superconducting element wires 11, 21, electrodes 12, 13 connected to both ends of the oxide superconducting element wire 11, and electrodes 22, 23 connected to both ends of the oxide superconducting element wire 21. Further, respective resistances Rs (Ω) between the oxide superconducting element wires 11, 21 and the respective electrodes 12, 13, and 22, 23 are made so that 0.01×0.01×10-6×L/Ic≤R≤5×0.01×10-6×L/Ic, where Ls (mm) are the lengths (mm) of the oxide superconducting element wires 11, 21 and Ic(A) is the critical current on a 0.01 μV/mm base in an external magnetic field of 0T.

COPYRIGHT: (C)2009,JPO&INPIT


Inventors:
Takashi Hase
Koji Shikimachi
Naoki Hirano
Shigeo Nagaya
Application Number:
JP2007206919A
Publication Date:
January 16, 2013
Filing Date:
August 08, 2007
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KABUSHIKI KAISHA KOBE SEIKO SHO
Chubu Electric Power Co., Inc.
International Classes:
H01F6/06; H01B12/02; H01B13/00
Domestic Patent References:
JP2003298129A
JP10050447A
JP2009043912A
JP2005322905A
JP2002540565A
Attorney, Agent or Firm:
Etsushi Kotani
Takao Ito
Muramatsu Toshiro



 
Previous Patent: JPS5118411

Next Patent: 鍋内溶鋼温度測定装置