Abstract:
A spring wire (20) with hardness of 50 to 56 HRC is subjected to first and second shot peening processes (S6) (S7) within a warm working temperature range of 150 to 350°C. In the first shot peening process (S6), the first shot of a shot size of 1.0 mm or more is used. In the second shot peening process (S7), the second shot smaller in shot size than the first shot is used. Through these shot peening processes (S6) (S7), compressive residual stress is imparted to the spring wire (20). The spring wire (20) includes a residual stress increase part (T1 residual stress peak part (T3), and residual stress decrease part (T4). In the residual stress decrease part (T4), a part (B) including the compressive residual stress magnitude of which is equivalent to the magnitude of the compressive residual stress at the surface of the spring wire (20) exists at a position at a depth exceeding the permissible pit depth (R max ).

Inventors:
Akira Tange
Hideki Okada
Sumiyoshi Isao
Mitsuhiro Sugiyama
Application Number:
JP2009144460A
Publication Date:
January 22, 2014
Filing Date:
June 17, 2009
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Nippon Jojo Co., Ltd.
International Classes:
B24C1/10; C21D7/06; F16F1/06
Domestic Patent References:
JP2008106365A
JP2004085685A1
JP2003055643A1
Attorney, Agent or Firm:
Suzue International Patent Office
Kurata Masatoshi
Satoshi Kono
Makoto Nakamura
Yoshihiro Fukuhara
Takashi Mine
Toshio Shirane
Sadao Muramatsu
Nobuhisa Nogawa
Kocho Chojiro
Naoki Kono
Katsu Sunagawa
Tetsuya Kazama
Katsumura Hiro
Shoji Kawai
Tatsushi Sato
Takashi Okada
Mihoko Horiuchi
Takenori Masanori
Takuzo Ichihara
Yamashita Gen



 
Previous Patent: JPS5393279

Next Patent: JPS5393281