Abstract:
The present invention provides activated carbon having excellent properties. The present invention consists of activated carbon, the key feature of which is an active surface area of at least 80 m2/g. In one preferred embodiment, the activated carbon consists of activated carbon fibers and is used for adsorption, and in a another preferred embodiment, the activated carbon also has a moisture adsorption rate (((mass B−mass A)/mass A)/×100%) of at least 40%, said moisture adsorption rate being determined from the mass (A) of the activated carbon after being dried for 24 hours at 115° C. and the mass (B) of the activated carbon after being kept for 24 hours in a thermo-hygrostat set to a temperature 25° C. and a relative humidity of 60%.
Inventors:
Junichi Yasumaru
Kojiro Tenno
Takenaka Shoichi
Hirohiko Tomura
Kojiro Tenno
Takenaka Shoichi
Hirohiko Tomura
Application Number:
JP2014526999A
Publication Date:
May 15, 2019
Filing Date:
July 25, 2013
Export Citation:
Assignee:
Kansai Thermochemical Co., Ltd.
Mc Evertech Co., Ltd.
Mc Evertech Co., Ltd.
International Classes:
C01B32/318; B01D53/28; B01J20/20; B01J20/28; C01B32/342
Domestic Patent References:
JP2004315243A | ||||
JP2012101948A | ||||
JP2011046584A | ||||
JP2009022931A | ||||
JP2002523329A | ||||
JP2118121A | ||||
JP2001180923A |
Other References:
安部郁夫,活性炭の製造方法,炭素,日本,炭素材料学会,2006年11月,Vol.2006, No.225,Page.373-381,ISSN:1884-5495,URL,https://doi.org/10.7209/tanso.2006.373
Attorney, Agent or Firm:
Asfi International Patent Office
Previous Patent: コンパクトで効率的な冷凍と適応性のある電源管理のための、極低温熱交...
Next Patent: 利用可能な帯域幅に応じてトランスポートプロトコルを選択することによ...
Next Patent: 利用可能な帯域幅に応じてトランスポートプロトコルを選択することによ...