Abstract:
PROBLEM TO BE SOLVED: To provide a heat treatment method for an α+β type titanium alloy capable of satisfying the characteristics required as those of a biomaterial while realizing precise dimensional shape, and an α+β titanium alloy product produced using the same.SOLUTION: Provided is a heat treatment method for a lamination-molded α+β type titanium alloy, comprising: a rapid heating step where heating is performed for 0.1 to 30 s at 800 to 1,200°C; and a rapid cooling step where, after the rapid heating step, cooling is performed at a cooling velocity of 40°C/s or higher.SELECTED DRAWING: Figure 3

Inventors:
TSUKAHARA MASAHIRO
FUKAZAWA KENGO
MISAKA YOSHITAKA
HISAMORI NORIYUKI
KIRIYAMA KENTARO
Application Number:
JP2015170767A
Publication Date:
March 09, 2017
Filing Date:
August 31, 2015
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NETUREN CO LTD
SOPHIA SCHOOL CORP
International Classes:
C22F1/18; B22F3/24; B33Y10/00
Domestic Patent References:
JPH11153140A1999-06-08
Attorney, Agent or Firm:
Katsuhiro Yoshimura
Kayo Ono