Abstract:
PROBLEM TO BE SOLVED: To provide an asphalt mixture capable of exhibiting a paved body capable of exhibiting strength in a relatively short time after application, also high in strength and durability and excellent in flexibility.SOLUTION: Provided is an asphalt mixture obtained by mixing an aggregate, asphalt, a lubricating solidification material and an alkaline additive, and the lubricating solidification material includes oleic acid in the ratio of 60 to 85 wt.%.SELECTED DRAWING: None
More Like This:
WO/2021/246871 | REJUVENATOR FOR RECYCLING OF POLYMER MODIFIED ASPHALT CONCRETE PAVEMENT |
JP2001270754 | PAVING MATERIAL |
Inventors:
MORIYASU HIROCHIKA
KOSHI KENTARO
TANIGUCHI HIROSHI
HATAKEYAMA KEIGO
KOSHI KENTARO
TANIGUCHI HIROSHI
HATAKEYAMA KEIGO
Application Number:
JP2015248258A
Publication Date:
June 29, 2017
Filing Date:
December 21, 2015
Export Citation:
Assignee:
MAEDA ROAD CONSTRUCTION CO LTD
International Classes:
C04B26/26; C04B24/08; C08K5/09; C08L95/00; E01C7/20
Attorney, Agent or Firm:
Eternal patent business corporation
Previous Patent: A manufacturing method and a manufacture device of a glass film layered product
Next Patent: A filler and a compound structure
Next Patent: A filler and a compound structure