Abstract:
There are provided an austenitic stainless steel having high stress corrosion crack resistance, characterized by containing, in percent by weight, 0.030% or less C, 0.1% or less Si, 2.0% or less Mn, 0.03% or less P, 0.002% or less S, 11 to 26% Ni, 17 to 30% Cr, 3% or less Mo, and 0.01% or less N, the balance substantially being Fe and unavoidable impurities; a manufacturing method for an austenitic stainless steel, characterized in that a billet consisting of the said austenitic stainless steel is subjected to solution heat treatment at a temperature of 1000 to 1150°C; and a pipe and a in-furnace structure for a nuclear reactor to which the said austenitic stainless steel is applied.

Inventors:
Yasuhiro Sakaguchi
Toshihiko Iwamura
Hiroshi Kanazaki
Hidehito Mimaki
Masaki Tanaike
Shunichi Suzuki
Kenro Takamori
Shun Oki
Naoki Aihara
Hiranuma Giju
Toshio Yonezawa
Application Number:
JP2005517050A
Publication Date:
January 19, 2011
Filing Date:
January 13, 2005
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
MITSUBISHI HEAVY INDUSTRIES,LTD.
THE TOKYO ELECTRIC POWER COMPANY,INCORPORATED
International Classes:
C22C38/00; C21D6/00; C21D6/02; C21D7/02; C21D8/00; C21D9/46; C22C38/58; G21C3/07; G21C13/08; G21D1/00
Domestic Patent References:
JPH0559494A1993-03-09
JPH07209485A1995-08-11
JPH0297651A1990-04-10
JP4014182B
Attorney, Agent or Firm:
Shoichi Okuyama
Arihara Koichi
Matsushima Tetsuo