To allow even fine inclusions to sufficiently float.
In the casting method for a continuous casting device, a tundish provided at the continuous casting device 1 is formed of a T type tundish 3 provided with a fluxing chamber 10 charged with a molten steel 2 from a ladle 9 and a distribution chamber 11 charging the molten steel 2 in the fluxing chamber 10 into a mold 4. The T type tundish 3 is provided with a partition gate 19 partitioning the fluxing chamber 10 and the distribution chamber 11 so as to optimize the shape of the partition gate 19, and further, a recessed part 17b is provided at the front wall 17 of the distribution chamber 11 facing the partition gate 19 so as to optimize the shape of the recessed part 17b. Casting is performed under casting conditions in accordance with the T type tundish having these shapes.
JP2008264859A | 2008-11-06 | |||
JP2009028776A | 2009-02-12 | |||
JP2005131661A | 2005-05-26 | |||
JPS6340652A | 1988-02-22 | |||
JP2008264859A | 2008-11-06 | |||
JP2009028776A | 2009-02-12 | |||
JP2005131661A | 2005-05-26 | |||
JPS6340652A | 1988-02-22 |
Mikio Yasuda
Next Patent: CASTING METHOD FOR CONTINUOUS CASTING DEVICE