Abstract:
A copper-nickel-tin alloy with excellent castability, hot and cold workability, high resistance to abrasive wear, adhesive wear and fretting wear and improved resistance to corrosion and stress relaxation stability, consisting of (in weight %): 2.0-10.0% Ni, 2.0-10.0% Sn, 0.01-1.5% Si, 0.01-1.0% Fe, 0.002-0.45% B, 0.001-0.15% P, selectively up to a maximum of 2.0% Co, optionally also up to a maximum 2.0% Zn, selectively up to a maximum of 0.25% Pb, the residue being copper and unavoidable impurities. The ratio Si/B of the element contents in wt. % of the elements silicon and boron is a minimum 0.4 and a maximum 8 such that the copper-nickel-tin alloy has Si-containing and B-containing phases, phases of the systems Ni—Si—B, Ni—B, Fe—B, Ni—P, Fe—P, Ni—Si, and other Fe-containing phases, which improve the processing and use properties of the alloy.

Inventors:
Webber Kai
Application Number:
JP2018565063A
Publication Date:
July 08, 2022
Filing Date:
June 27, 2017
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
WIELAND-WERKE AKTIENGESELLSCHAFT
International Classes:
C22C9/06; C22C9/02; C22F1/08
Domestic Patent References:
JP3115538A
Foreign References:
US6379478
US2129197
Attorney, Agent or Firm:
Akiyoshi Sato