To provide a curing composition for an antireflection film of a microlens to obtain a cured film having a high refractive index and excellent light resistance, and to provide an antireflective layered product for a microlens by using the above composition.
The curing composition for an antireflection film of a microlens contains: (A) 100 parts by weight of titanium oxide particles coated with an oxide of one or more metal elements selected from a group comprising silicon, aluminum, titanium, zirconium, tin, antimony and zinc; (B) 1 to 300 parts by weight of a curing compound; and (C) 0.1 to 60 parts by weight of a curing catalyst. The antireflective layered product for a microlens including a cured film obtained from the above composition shows excellent antireflection property.