Title:
FINE FIBROUS CELLULOSE
Document Type and Number:
Japanese Patent JP2016199770
Kind Code:
A
Abstract:
PROBLEM TO BE SOLVED: To provide a fine fibrous cellulose which is low in viscosity when slurried and prevents an aggregate from being formed when mixed with an emulsion resin.SOLUTION: A fine fibrous cellulose has an average fiber width of 200 nm or less and a degree of polymerization of 50 or more and 500 or less, has a polar group represented by formula (1): (-O-PO) Xand a polar group represented by formula (2): (-OCO-R-COO)Y, and has a content of the polar group of 0.06-2.0 mmol/g. In formulae (1) and (2), p is 1 or 2; and q is a natural number of 1 to 3.SELECTED DRAWING: None
More Like This:
JP7188229 | Method for producing fibrous cellulose-containing slurry |
JP2020172461 | POWDERY LIQUID |
WO/2018/143149 | PRODUCTION METHOD OF DRIED CELLULOSE NANOFIBERS |
Inventors:
NOGUCHI YUICHI
NOISHIKI YASUTOMO
NOISHIKI YASUTOMO
Application Number:
JP2016174155A
Publication Date:
December 01, 2016
Filing Date:
September 07, 2016
Export Citation:
Assignee:
OJI HOLDINGS CORP
International Classes:
C08B5/00; C08B3/12
Domestic Patent References:
JP2009293167A | 2009-12-17 | |||
JP2005511797A | 2005-04-28 | |||
JP2008024778A | 2008-02-07 | |||
JP2008034556A | 2008-02-14 | |||
JP2013253200A | 2013-12-19 |
Previous Patent: 基板処理装置及び基板処理方法
Next Patent: A manufacturing method and a molding thing of composite fuel
Next Patent: A manufacturing method and a molding thing of composite fuel