Abstract:

PURPOSE: The titled composition that is obtained by admixing appropriately the following essential components: SiO2, B2O3, Al2O3 and Cu2O, thus being suitably used as an insulating coat under the load of large tensile stress.

CONSTITUTION: The objective glass composition is composed of, as essential components, 30W65mol% of SiO2, 11W45mol% of B2O3, 5W15mol% of Al2O3, and 10W20mol% of Cu2O and, as optional components, less than 5mol% of P2O5, less than 2mol% of V2O5, less than 2mol% of Na2O, less than 5mol% of PbO, less than 3mol% of SnO2 and less than 10mol% of ZnO. The total amounts of the essential components are required to exceed 85mol%. The resultant composition has a softening point of about up to 660°C and a thermal expansion coefficient of less than 40×10-17/°C. The composition is suitably used as an insulating coat formed on silicon steel plates.


Inventors:
OKUYAMA MASAHIKO
KONDOU KAZUO
SHIBATA YOSHIMASA
Application Number:
JP14406483A
Publication Date:
February 25, 1985
Filing Date:
August 05, 1983
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NGK SPARK PLUG CO
International Classes:
C03C3/064; C03C3/091; C03C3/097; C03C3/108; C03C4/16; H01B3/08; (IPC1-7): C03C3/064; C03C3/091; C03C3/097; C03C3/108; C03C4/16; H01B3/08
Domestic Patent References:
JP43025205A