Abstract:
To provide a high-strength low-alloyed titanium alloy having a tensile strength of ≥750 MPa, and a production method which can produce such a titanium alloy using an inexpensive, low-quality sponge titanium as a raw material.
The high-strength low-alloyed titanium alloy has an alloy composition comprising 0.2-0.8% O, 0.01-0.15% C, 0.01-0.07% N, 0.3-1.0% Fe and the balance substantially being Ti. When producing this, the low-quality Ti sponge containing ≥0.01% N and ≥0.2% Fe is used as a part of the raw material as sources of N and Fe components.
Inventors:
SUZUKI AKIHIRO
KAMIYA HISAO
HORIMURA HIROYUKI
DOI KOUSUKE
KAMIYA HISAO
HORIMURA HIROYUKI
DOI KOUSUKE
Application Number:
JP2003063717A
Publication Date:
September 30, 2004
Filing Date:
March 10, 2003
Export Citation:
Assignee:
DAIDO STEEL CO LTD
HONDA MOTOR CO LTD
HONDA MOTOR CO LTD
International Classes:
C22F1/18; C22C14/00; C22F1/00; (IPC1-7): C22C14/00; C22F1/18
Domestic Patent References:
JPH01252747A | 1989-10-09 | |||
JPH08295969A | 1996-11-12 | |||
JP2001089821A | 2001-04-03 | |||
JPH1136029A | 1999-02-09 | |||
JPH09154854A | 1997-06-17 |
Foreign References:
WO1996033292A1 | 1996-10-24 |
Attorney, Agent or Firm:
Sooo Suga
Previous Patent: PRODUCTION METHOD OF STEEL BAR
Next Patent: SURFACE TREATMENT DEVICE AND SURFACE TREATMENT METHOD
Next Patent: SURFACE TREATMENT DEVICE AND SURFACE TREATMENT METHOD