A process is provided for welding a nickel or cobalt based superalloy article to minimize cracking by preheating the entire weld area to a maximum ductility temperature range, maintaining such temperature during welding and solidification of the weld, raising the temperature for stress relief of the superalloy, then cooling at a rate effective to minimize gamma prime precipitation.

Inventors:
Foster michael
Up De Grove, Kevin
Application Number:
JP2001583972A
Publication Date:
July 04, 2012
Filing Date:
February 21, 2001
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Chromaloy Gas Turbine Corporation
International Classes:
B23K31/00; F02C7/00; B23K9/23; B23K20/00; B23K26/34; B23K28/02; B23K9/04; B23K35/30; B23K103/08
Domestic Patent References:
JP5192785A
JP6218573A
JP7145703A
JP8170132A
JP9506039A
JP10510323A
JP2000042755A
Attorney, Agent or Firm:
Kazuo Shamoto
Tadashi Masui
Yasushi Kobayashi
Akio Chiba
Hiroyuki Tomita
Shigeru Sakuma



 
Previous Patent: JPS4969755

Next Patent: JPS4969757