To provide a hydrated hardened body having a reinforcing rod excellent in neutralization resistance and salt damage resistance which can made into a structure member having durability over a long period even under environmental conditions that neutralization is apt to progress.
The hydrated hardened body, which has the reinforcing rod excellent in neutralization resistance and salt damage resistance at the inside, at least contains: steel making slag; blast furnace slag fine powder; and fly ash, and in which the fly ash content is ≥100 kg/m
COPYRIGHT: (C)2008,JPO&INPIT
MATSUNAGA HISAHIRO
KYONO KAZUAKI
JP2003165751A | 2003-06-10 | |||
JP2004051426A | 2004-02-19 | |||
JP2004149333A | 2004-05-27 | |||
JP2001163656A | 2001-06-19 | |||
JP2005145747A | 2005-06-09 | |||
JP2002068804A | 2002-03-08 | |||
JP2004299922A | 2004-10-28 | |||
JP2003055025A | 2003-02-26 | |||
JP2004051425A | 2004-02-19 | |||
JP2003306359A | 2003-10-28 | |||
JPH08134587A | 1996-05-28 | |||
JPH1180880A | 1999-03-26 | |||
JPH1121622A | 1999-01-26 | |||
JPH0740331A | 1995-02-10 | |||
JP2002059076A | 2002-02-26 |
Kazuhiro Mori