To discourage crackings caused by difference in contraction behavior between an internal electrode and a ceramic layer, inside a laminate at baking.
A laminated body 3, where a ceramic layer 7 and internal electrodes 5 and 6 are laminated alternately and external electrodes 2 and 2 are provided at the end part of the laminated body 3, are provided. The internal electrodes 5 and 6 reach at least either of pair of edges of the ceramic layer 7, which face each other so that the internal electrodes 5 and 6 are led out to a facing end surface of the laminate 3, with the internal electrodes 5 and 6 being lead out to the end surface of the laminate 3 connected, respectively to the external electrodes 2 and 2. At the internal electrodes 5 and 6, facing each other inside the laminate 3 via the ceramic layer 7, a void part where partially no conductor particle ceramic particle exists is provided.