To provide a lithium-ion secondary battery which can stably maintain charging/discharging capacity over a long period of time, while increasing rapid charging capacity.
A lithium-ion secondary battery 10 comprises: an internal electrode pair 1 obtained by alternately laminating a sheet-shaped positive electrode 1a using lithium metal oxide as positive pole active material 12 and a sheet-shaped negative electrode 1b using lithium titanium oxide as negative pole active material 14, via a separator 1c; and an exterior body for storing the internal electrode pair 1 together with an electrolytic solution DL in a sealed state. In the battery, the capacity of the negative pole active material 14 is set at a value smaller than that of the positive pole active material, and the press density of the negative pole active material 14 is 1.4-1.7 g/cc.
SUGAWARA SHUICHI
FUJISAKI TAKASHI
OZAWA KAZUNORI
JP2010009898A | 2010-01-14 | |||
JP2009277395A | 2009-11-26 | |||
JP2004071405A | 2004-03-04 | |||
JPH1027626A | 1998-01-27 | |||
JP2000012090A | 2000-01-14 | |||
JPH1069922A | 1998-03-10 | |||
JP2007273166A | 2007-10-18 | |||
JP2008511528A | 2008-04-17 | |||
JP2006253081A | 2006-09-21 | |||
JP2007227090A | 2007-09-06 | |||
JP2010153258A | 2010-07-08 | |||
JP2007323958A | 2007-12-13 | |||
JP2009245762A | 2009-10-22 | |||
JP2011091039A | 2011-05-06 | |||
JP2010009898A | 2010-01-14 | |||
JP2009277395A | 2009-11-26 | |||
JP2004071405A | 2004-03-04 | |||
JPH1027626A | 1998-01-27 | |||
JP2000012090A | 2000-01-14 | |||
JPH1069922A | 1998-03-10 | |||
JP2007273166A | 2007-10-18 | |||
JP2008511528A | 2008-04-17 | |||
JP2006253081A | 2006-09-21 | |||
JP2007227090A | 2007-09-06 | |||
JP2010153258A | 2010-07-08 | |||
JP2007323958A | 2007-12-13 | |||
JP2009245762A | 2009-10-22 |
Katsuo Naruse
Tomohiro Nakamura