Abstract:
PROBLEM TO BE SOLVED: To provide a magnetic core in which peeling, dropping or cracking of a flat power is less likely to occur with a ridge line part of an end face or a corner part to which the ridge line part is matched, defined as an origin, an inductor, and a manufacturing method thereof.SOLUTION: The present invention relates to a magnetic core consisting of a flat soft magnetic metal powder in 60 vol.% or more, a binder containing silicon nitride in 10 vol.% or more and 30 vol.% or less as a main component, and a compound magnetic substance including pores in 10 vol.% or more and 25 vol.% or less, being elastic and having a polygonal shape. A ridge line part and a corner part are rounded and an end of the soft magnetic metal powder in the rounded portion is folded.SELECTED DRAWING: Figure 2

Inventors:
Ken'ichi Chatani
Mikoshiba Hayao
Hiroshi Shima
Hiroyuki Kamada
Application Number:
JP2017005750A
Publication Date:
March 31, 2021
Filing Date:
January 17, 2017
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
Tokin Co., Ltd.
International Classes:
H01F27/255; H01F1/24; H01F3/08; H01F41/02
Domestic Patent References:
JP2014168038A
JP2016171160A
JP2013051276A
JP8213719A
JP6325978A
JP2005269599A
JP2012129352A
Attorney, Agent or Firm:
Kenho Ikeda
Takashi Sasaki