Title:
MANUFACTURE OF NORMALIZED STEEL PLATE PREVENTABLE FROM WELD CRACKING
Document Type and Number:
Japanese Patent JPS5387920
Kind Code:
A
Abstract:
PURPOSE: To manufacture a homogeous steel plate with sufficient strength by carrying out spray cooling after normalizing as well as decreasing the contents of alloy components so as to lower weld sensibility index and carbon equivalent.
More Like This:
WO/1997/026379 | READY-TO-USE METAL WIRE AND METHOD FOR PRODUCING SAME |
Inventors:
HAGIWARA YASUHIKO
YOSHINAGA HISASHI
TSUGAI HIROMICHI
YASUKAWA SHIYOUZOU
TAKEUCHI OSAMU
KOKUBU HARUO
YOSHINAGA HISASHI
TSUGAI HIROMICHI
YASUKAWA SHIYOUZOU
TAKEUCHI OSAMU
KOKUBU HARUO
Application Number:
JP327177A
Publication Date:
August 02, 1978
Filing Date:
January 13, 1977
Export Citation:
Assignee:
SUMITOMO METAL IND
ISHIKAWAJIMA HARIMA HEAVY IND
ISHIKAWAJIMA HARIMA HEAVY IND
International Classes:
C21D9/52; C21D1/28; C21D6/00; (IPC1-7): C21D6/00
Domestic Patent References:
JPS5227087A | 1977-03-01 |
Previous Patent: JPS5387919
Next Patent: GRAIN REFINING METHOD FOR AUSTENITE IN FERRITICAUSTENITIC TWO-PHASES TAINLESS STEEL
Next Patent: GRAIN REFINING METHOD FOR AUSTENITE IN FERRITICAUSTENITIC TWO-PHASES TAINLESS STEEL