Abstract:
To provide a method for manufacturing a positive active material for a nonaqueous secondary battery having high capacity at least similar to the conventional active material simply even in a device and operation.
In the manufacturing method of the positive active material for the nonaqueous secondary battery by baking a mixture of metal element compounds, the mixture obtained by conducting mixing, drying, and crushing at the same time with crushing media and a vibration dryer, and preferably, mixing, drying and crushing are conducted in a state in which no places condensing moisture are present in the vibration dryer.
More Like This:
Inventors:
Shioda, Katsuyuki
Kawakami, Yoshihiro
Kawakami, Yoshihiro
Application Number:
JP2006000344189
Publication Date:
July 10, 2008
Filing Date:
December 21, 2006
Export Citation:
Assignee:
SUMITOMO CHEMICAL CO LTD
International Classes:
H01M4/58; H01M4/02
Previous Patent: POWER SOURCE SYSTEM
Next Patent: BATTERY DETERIORATION SUPPRESSION METHOD, BATTERY STORAGE CHAMBER, AND ELECTRONIC EQUIPMENT
Next Patent: BATTERY DETERIORATION SUPPRESSION METHOD, BATTERY STORAGE CHAMBER, AND ELECTRONIC EQUIPMENT