To provide a material for a coating of a curing type solvent-based soft feeling coating capable of obtaining a soft touch feeling even by using a normal coating method or film thickness, and a coating and coated film by using such the material.
This material for the curing type solvent-based soft feeling coating is provided by comprising a lipophilic polyrotaxane having a ring molecule, a straight chain molecule and blocking groups, wherein, the straight chain molecule and ring molecule each has a hydrophobic modifying group. The inclusion amount of the ring molecule is 0.06-0.61. The molecular weight of the straight chain molecule is 1,000-100,000. The curing type solvent-based soft feeling coating is obtained by using the material for the curing type solvent-based soft feeling coating. The solvent-based clear coated film is obtained by solidifying the curing type solvent-based soft feeling coating. The laminated coated film is provided by forming the soft feeling coated film on a material to be coated.
ARAKI JUN
SUZUKI TATSUYA
YAMANAKA MASAHIKO
WATANABE KENTARO
UNIV TOKYO
JP2007099994A | 2007-04-19 | |||
JP2007099995A | 2007-04-19 | |||
JP2005075979A | 2005-03-24 | |||
JP2005143920A | 2005-06-09 | |||
JP2007091938A | 2007-04-12 | |||
JP2007099988A | 2007-04-19 | |||
JP2007099989A | 2007-04-19 | |||
JP2007099990A | 2007-04-19 | |||
JP2007099992A | 2007-04-19 | |||
JP2007099993A | 2007-04-19 |
WO2003074099A1 | 2003-09-12 |