Abstract:
To provide a grout composition which is excellent in fluidity, compensates the settling or shrinkage of unhardened mortar or concrete and is excellent in initial strength development and dimensional stability even in a cold season of around 5°C and to provide mortar or concrete and a grout material using the mortar or concrete.
The grout composition (1) contains: a hydraulic material containing a 3Ca-SiO2solid solution, 11CaO-7Al2O3-CaF2and anhydrous gypsum; a quick hardening material containing calcium aluminosilicate glass and anhydrous gypsum; fine powder of blast furnace granulated slag; silica fume; calcium hydroxide; alkali metal aluminate; a high-performance water reducing agent; and a setting modifier. The grout composition (2) is the grout composition (1), containing a polycarboxylic acid-based high-performance water reducing agent and a melamine-based high-performance water reducing agent as the high-performance water reducing agent. The grout composition (3) is the grout composition (1) or the grout composition (2), containing calcium nitrite and/or calcium nitrate. Mortar or concrete is obtained by blending the grout composition, water and aggregate.
COPYRIGHT: (C)2008,JPO&INPIT
Inventors:
Minoru Morioka
Satoshi Takagi
Akio Takahashi
Application Number:
JP2006089928A
Publication Date:
October 17, 2012
Filing Date:
March 29, 2006
Assignee:
DENKI KAGAKU KOGYO KABUSHIKI KAISHA
International Classes:
C04B28/02; C04B7/345; C04B18/14; C04B22/02; C04B22/06; C04B22/08; C04B22/14; C04B24/06; C04B24/26; C04B24/30; C09K17/44; E02D3/12; C04B111/70; C04B111/72; C09K103/00
Domestic Patent References:
JP200627937A | | | | |
JP60108352A | | | | |
JP63206336A | | | | |
JP2005271280A | | | | |
JP2005170710A | | | | |
JP2672004B2 | | | | |
JP11207727A | | | | |
JP2005289656A | | | | |
JP11130498A | | | | |
JP1294554A | | | | |
JP2000143314A | | | | |
JP2000247716A | | | | |