To provide a method for manufacturing an inkjet recording medium capable of obtaining high printing density and suppressing coating defects.
The method for manufacturing the inkjet recording medium includes a process of applying: at least a coating liquid A containing a vapor-phase-process silica and a water-soluble binder; a coating liquid B containing a pseudo boehmite alumina hydrate, in which the content of water-soluble binder with respect to the content of the pseudo boehmite alumina hydrate and the content of a crosslinking agent with respect to the content of the pseudo boehmite alumina hydrate are respectively less than 3 mass%; and a coating liquid C containing the crosslinking agent, in this order on a support body from the support body side to form an ink receiving layer.