To provide a method for manufacturing a bearing ring, which can uniformly form a quench-hardened layer in the whole rolling face along the perimeter by induction hardening while suppressing a manufacturing cost of a quenching apparatus.
The method for manufacturing the bearing ring of a rolling bearing includes: a step (S10) of preparing a molded body which is constituted by a steel including 0.43-0.65% carbon, 0.15-0.35% silicon, 0.60-1.10% manganese, 0.30-1.20% chromium, 0.15-0.75% molybdenum and the balance iron with impurities; a step (S30) of relatively rotating an induction-heating member along the circumferential direction of an annular region, which is arranged so as to face a part of the annular region that becomes the rolling face of the bearing ring in the molded body and induction-heats the molded body to form an annular heated region which has been heated to a temperature of a point A
COPYRIGHT: (C)2011,JPO&INPIT
Kazuhiro Yagita
Takashi Yuki
JP2008303402A | ||||
JP4000349A | ||||
JP60145324A | ||||
JP2004100946A | ||||
JP2009156295A | ||||
JP2009197312A | ||||
JP2005133123A | ||||
JP2004044802A |
Toshio Morita
Yoshihei Nakamura
Yutaka Horii
Masayuki Sakai
Nobuo Arakawa
Masato Sasaki