To monitor stress changes in a long period on stress measurement on a member to be measured, a structure made of a nonmagnetic material.
A measuring plate 2 made of a magnetic body is pasted to the member to be measured 1 made of a nonmagnetic material, and distortion of the measuring plate 2 is converted into stress by a magnetostrictive method to measure stress of the member to be measured 1. Stress immediately after the measuring plate 2 is pasted to the member to be measured 1 or before the pasting is measured by a magnetostrictive method and taken as initial stress. Stress of the measuring plate 2 after load of the member to be measured 1 is changed is measured by a magnetostrictive method, and the difference between the result of stress measurement after the load of the measuring plate 2 is changed and the initial stress is taken as stress of the member to be measured 1.
FUJIOKA YASUHIRO
ODA TAKUYA
IWAGAMI AKIRA
ARITSUNE TAKESHI
YASUFUKU SEIICHI
CHUGOKU ELECTRIC POWER
Field saki Akira
Next Patent: REFERENCE HOLDER FOR ROUNDNESS MEASURING MACHINES