To provide a nitriding method by which nitrogen atoms can be rapidly and uniformly incorporated from the surface layer of a steel component down into its deep part.
The nitriding method comprises heating the steel component in a gaseous nitriding treatment atmosphere, solidfying the nitrogen atoms contained in the nitriding treatment gas onto the surface of the steel component, and diffusing the solidified nitrogen atoms into the steel component. The treatment method performs the nitriding treatment while maintaining the heating temperature of the nitriding treatment at ≥590°C and lowering the concentration of the nitriding treatment gas lower thanr that of the nitriding treatment gas at the start of the nitriding treatment.