To provide a photocatalytic body which photocatalytic particles strongly adhere over a long period of time without losing ability with extremely little degradation and deterioration of the binder caused by the photocatalytic particles.
A photocatalytic body keeps a first layer containing a persistent binder overlying a substrate, but no photocatalytic particles, and the first layer is costed or sprayed with a mixture of the persistent binder and the photocatalytic particles and dried at an ambient temperature of 200°C to provide a second layer. The volume of photocatalytic particles as a volume standard against a total amount of the photocatalytic particles and the persistent binder of the second layer is; (1) 5-40%, if the persistent binder is cement and/or gypsum, (2) 20-98%, if the persistent binder is not cement and/or gypsum.
COPYRIGHT: (C)2008,JPO&INPIT
MURAKAMI HAJIME
FUKUI YASURO
WATANABE MITSURU
FUJISHIMA AKIRA
HASHIMOTO KAZUHITO
FUJISHIMA AKIRA
HASHIMOTO KAZUHITO
TOTO LTD
JPH06327965A | 1994-11-29 | |||
JPH05253544A | 1993-10-05 | |||
JPH04284851A | 1992-10-09 | |||
JPH04174679A | 1992-06-22 | |||
JPH02273514A | 1990-11-08 | |||
JPH01218635A | 1989-08-31 |
Hajime Asamura
Kajiwara Saiko
Yukihiro Ikeda
Next Patent: METHOD FOR DECOMPOSING FLUORESCENT BRIGHTENING AGENT