To obtain a positive electrode material for LiNiO
A slurry, which consists of a particle having a hydroxide obtained by mixing a water solution of a nitrate of nitric acid zirconium oxide in addition to nickel nitrate and other metal nitrate as a main component, and a water solution of lithium hydroxide and a water solution phase having as a main component a nitrate, is sprayed and dried in high temperatures, and a precursor of granular lithium transition metal compound oxide having two phases of a hydroxide phase and a nitrate phase is formed. By calcining (tentative calcination and final calcination) the precursor, a lithium transition compound oxide having a Hardgrove grindability index of 90 or more is formed, and by crushing this, LiNiO