Abstract:

PURPOSE: To obtain coal slurry having such viscosity that it can be transported by pipeline, by blending coal particles adjusted to particle diameters in a specific range with a liquid to give slurry having a specific concentration.

CONSTITUTION: Coal particles having 5W95wt% cumulative weight ratio, having a particle size distribution adjusted in such a way that it obeys the formula [D is coal particle diameter(μm); D50 is coal particle diameter(μm)(5W500μm) at 50wt% cumulative weight ratio; F is cumulative weight ratio(wt%) of coal particle finer than coal particle diameter D; a is 2W5 in ≥D50 particle diameter range, and 1W3 in ≤D50 range particle diameter range] is blended with a liquid such as water, petroleum oil, methanol, etc. and the coal concentration is adjusted to ≥55wt%, to give the desired slurry.


Inventors:
Kaji, Ryuichi
Muranaka, Tadashi
Kikuchi, Hideo
Noguchi, Yoshiki
Application Number:
JP1983000125789
Publication Date:
January 30, 1985
Filing Date:
July 11, 1983
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
HITACHI LTD
BABCOCK HITACHI KK
International Classes:
C10L1/32; (IPC1-7): C10L1/32