To obtain a solidified fuel which does not generate dioxins and is excellent in deodorizing and antibacterial properties by compounding at least either a baked dolomite or dolomite.
Preferably, a baked dolomite and/or dolomite is compounded in an amount of 5-15 wt.% of the resultant solidified fuel, The particle size of the baked dolomite or dolomite is 1 mm or lower, A baked dolomite prepared by baking dolomite at 900-1,200°C is preferable, For example, after crushed, sorted and dried, a waste as the raw material is compounded with a baked dolomite and/or dolomite and molded; after crushed and sorted, the raw material is compounded with a baked dolomite and/or dolomite, molded and dried; or after crushed and sorted, the raw material is compounded with a baked dolomite and/or dolomite, dried and molded.
MOCHISE DENKI KK
SUMIYOSHI KINZOKU KK