To provide a spring that has excellent fatigue resistance, reduces material costs and simplifies manufacturing processes.
A method for manufacturing the spring includes: a shaping step of shaping a wire rod having components consisting of, by mass, 0.5-0.7% of C, 1.0-2.0% of Si, 0.1-1.0% of Mn, 0.1-1.0% of Cr, 0.035% or less of P,0.035% or less of S, and the balance Fe and inevitable impurities, into a spring shape; a thermal treatment step of austenizing the spring at the temperature of Ac3 point or more (Ac3 point+250°C), and then cooling the spring at the rate of 20°C/sec or more, holding the spring for 400 sec or more at the temperature of (Ms point-20°C) to (Ms point+60°C), and cooling the spring to a room temperature; and a shot peening step of projecting a shot at the heat treated spring.
ONO YOSHIKI
KUROKAWA SHINPEI
SHIBAIRI KOSUKE
JPH02129422A | 1990-05-17 | |||
JPH1180895A | 1999-03-26 | |||
JP2007154240A | 2007-06-21 | |||
JP2006291291A | 2006-10-26 | |||
JP2001220650A | 2001-08-14 | |||
JPS63312917A | 1988-12-21 | |||
JPH02129422A | 1990-05-17 | |||
JPH1180895A | 1999-03-26 | |||
JP2007154240A | 2007-06-21 | |||
JP2006291291A | 2006-10-26 | |||
JP2001220650A | 2001-08-14 | |||
JPS63312917A | 1988-12-21 |
WO2010110041A1 | 2010-09-30 | |||
WO2010110041A1 | 2010-09-30 |
Next Patent: ATOMIZATION DEVICE