To improve external appearance, strength, elastic modulus and impact strength of a molded product by heating and pressurizing a composite laminate having thermoplastic resin layers laminated via organic peroxide layers on both surfaces of glass fiber paper body containing thermoplastic resin, and molding it in a sheet-like article.
Organic peroxide layers 12a, 12b are provided on both surfaces of glass fiber paper body 11. Further, thermoplastic resin layers 13a, 13b made of thermoplastic resin films are laminated on surfaces of the layers 12a, 12b. The composite laminate has thermoplastic resin thin layers made of thin thermoplastic resin films laminated between the layer 12a and the paper body 11 and between the layer 12b and the paper body 11. Since the thermoplastic resin thin layers are laminated between the organic peroxide layer and the medium, the molded product having excellent external appearance can be obtained by flow molding.
UCHIDA YUICHI
NAGASHIMA YUKIO
YOSHIKAWA FUMIAKI
Next Patent: DEHYDRATING AND DRYING OF EP(D)M