Abstract:
A storage-stable modified asphalt composition, which comprises: 50-97.7 parts by weight of a base asphalt, 2.0-20.0 parts by weight of a polymer having double bonds, 0.1-20.0 parts by weight of a compatibilizer, 0.1-10.0 parts by weight of a cross-linking reagent, and 0.1-10.0 parts by weight of a organic polar compound, and the softening point difference of its product determined by the stability test is lower than 2.5° C. The process for preparing said modified asphalt composition is mixing 50-97.7 parts by weight of a base asphalt, 2.0-20.0 parts by weight of a polymer having double bonds, 0.1-20.0 parts by weight of a compatibilizer 0.1-10.0 parts by weight of a cross-linking reagent, and 0.1-10.0 parts by weight of a organic polar compound under certain conditions. The modified asphalt provided by the present invention has good storage-stability. The preparation process provided by the present invention is simple, and there is no need for special apparatus.

Inventors:
Guo Shuhua
Yellow prayer
Dragon army
Zhang Hyakuharu
Prince army
Yu Tamari
Application Number:
JP2001249485A
Publication Date:
October 22, 2008
Filing Date:
August 20, 2001
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
China Petrochemical Co., Ltd.
China Petrochemical Co., Ltd. Petrochemical Research Institute
International Classes:
C08L95/00; E01C7/18; C08J3/20; C08K3/00; C08K3/06; C08K3/32; C08K5/00; C08K5/07; C08K5/09; C08K5/17
Foreign References:
WO1998047966A1
Attorney, Agent or Firm:
Ikeuchi, Sato & Partners