To provide a tube container which is excellent in flexibility, transparency and surface glossiness.
The tube container includes a propylene-based resin which has an MFR of 2.0 to 40 g/10min or less, a DSC melting point of 100 to 145 °C, a tensile modulus of 100 to 600 MPa, and a haze of 2 mmt injection square plate of 65% or less or a propylene random copolymer (B) which has an MFR of 2.0 to 40 g/10 min, and a DSC melting point of 100 to 145 °C and satisfies the following requisites (b1) and (b3), and a propylene copolymer rubber (C) which has an MFR of 0.1 to 50 g/10min and satisfies the following requisites (c1) to (c3): (b1) the content of skeleton derived from ethylene is 0.5 mol% or more and less than 14 mol%; (b3) the DSC melting point is 100 to 145°C; (c1) the density is 860 to 890 kg/m3; (c2) the shore A hardness is 60 to 80; and (c3) the DSC melting point is 120 to 150 °C.