To provide an improved method for the preparation of cellulose powder which provides easy handling and high output of cellulose powder with desired particle size.
A screen comprising at least two layers of different mesh or pore size is used in a cellulose powder preparation method. The screen has one screening layer and one supporting layer providing mechanical stability to the screening layer, wherein the mesh or pore size of the screening layer is less than 250 μm, and the screening layer has a coarser mesh or pore size than the screening layer, the mesh or pore size ratio of the two layers is from 1.05:1 to 30:1, the screening layer is sintered to the supporting layer, the two layers are inseparable from each other over the whole area, and cellulose is sieved in dry state.
SCHNEIDER HANS-PETER
MERZ GUNNAR R
KRUSE PETER
JP2006053515A | 2006-02-23 | |||
JPS63130173U | 1988-08-25 | |||
JPH01217001A | 1989-08-30 | |||
JPH0217530U | 1990-02-05 | |||
JPH08131875A | 1996-05-28 | |||
JPH06136001A | 1994-05-17 | |||
JPH01217001A | 1989-08-30 |
Takashi Ishida
Tetsuji Koga
Nagasaka Tomoyasu
Yoshihiro Kobayashi
Atsushi Ebiya
Next Patent: WATER PURIFIER AND METHOD FOR CLEANING THE SAME