Title:
WELD FILLER FOR SUPERALLOYS
Document Type and Number:
Japanese Patent JP2016117099
Kind Code:
A
Abstract:
PROBLEM TO BE SOLVED: To provide a weld filler metal for superalloys.SOLUTION: A weld filler metal for a superalloy for welding is disclosed. The weld filler metal includes a preformed article that contains a first material with a melting point of approximately 2300 to 2500°F, and a second material with a melting point of approximately 1800 to 2200°F, where the proportion of the first material to the second material is variable. Related processes and articles are also disclosed.SELECTED DRAWING: Figure 1
More Like This:
Inventors:
SRIKANTH CHANDRUDU KOTTILINGAM
CUI YAN
LIN DECHAO
DAVID EDWARD SCHICK
TOLLISON BRIAN LEE
CUI YAN
LIN DECHAO
DAVID EDWARD SCHICK
TOLLISON BRIAN LEE
Application Number:
JP2015240683A
Publication Date:
June 30, 2016
Filing Date:
December 10, 2015
Export Citation:
Assignee:
GENERAL ELECTRIC CO GE
International Classes:
B23K35/30; B22D19/10; B23K9/00; B23K9/167; B23K9/23; B23K10/02; B23K15/00; B23K26/32; B23K31/00; B23P6/04; C22C19/05; C22C19/07; C22C30/00; F01D5/28; F01D25/00; F02C7/00
Domestic Patent References:
JPH07500539A | 1995-01-19 | |||
JP2011033028A | 2011-02-17 | |||
JP2001179432A | 2001-07-03 | |||
JPS6453797A | 1989-03-01 |
Foreign References:
US20140212681A1 | 2014-07-31 | |||
US20060216540A1 | 2006-09-28 |
Attorney, Agent or Firm:
Arakawa Satoshi
Hirokazu Ogura
Toshihisa Kurokawa
Takuto Tanaka
Hirokazu Ogura
Toshihisa Kurokawa
Takuto Tanaka