Abstract:
Disclosed is an alloy drill. Components of the alloy drill are: 14-30 wt% of a binder phase being one or more of Co, Ni, Fe, and Cu; 0.32-9.7 wt% of an additive being one or more of TaC, MoC, Cr3C2, and MnC; and the remainder as a hard phase being WC. In the alloy drill, WC is used as the hard phase to improve its hardness and wear resistance, Cu, Ni, Fe, or Co as the binder phase can improve its anti-corrosion performance and anti-fatigue performance, and TaC, MoC, Cr3C2, or MnC as the additive can further improve its thermal stability and wear resistance. Thus, the alloy drill has superior wear resistance and impact toughness, and also possesses excellent anti-corrosion performance and anti-fatigue performance.

Inventors:
LIU BIN (CN)
XU YUEHUA (CN)
WU JI (CN)
CAO ZHIHUA (CN)
Application Number:
PCT/CN2015/095050
Publication Date:
May 04, 2017
Filing Date:
November 19, 2015
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
SEED TECH CORP LTD (CN)
International Classes:
C22C29/08; C22C1/05; E21B10/46
Domestic Patent References:
WO1994015740A11994-07-21
Foreign References:
CN103614604A2014-03-05
CN103266249A2013-08-28
JP2002120104A2002-04-23
Attorney, Agent or Firm:
UNITALEN ATTORNEYS AT LAW (CN)
Download PDF: