ALLOY HAVING HIGH CORROSION RESISTANCE IN ENVIRONMENT OF HIGH CORROSIVENESS, STEEL PIPE OF THE SAME ALLOY AND METHOD OF MANUFACTURING THE SAME STEEL PIPE
Document Type and Number:
WIPO Patent Application WO/1997/039153
Kind Code:
A1
Abstract:
An alloy of a high corrosion resistance used for a steel pipe for a boiler in equipment in which a fossil fuel or waste matter is burnt to generate energy, a steel pipe using this alloy, and a method of manufacturing the same steel pipe are provided. An alloy comprising not more than 0.05% of C, 1.0-2.6% of Si, 0.02-1.0% of Mn, 20.0-28.0% of Cr, 18.0-30.0% of Ni, not more than 4.0% of Mo, not more than 0.05% of Al, 0.05-0.30% of N, and the rest comprising Fe and unavoidable impurities. A double-layer steel pipe comprising a steel pipe for a standardized boiler as a base layer member, and this alloy as a material for a liner member; and a method of manufacturing the same steel pipe.

Inventors:
ISHITSUKA TETSUO (JP)
NOSE KOICHI (JP)
Application Number:
PCT/JP1997/001302
Publication Date:
October 23, 1997
Filing Date:
April 15, 1997
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NIPPON STEEL CORP (JP)
ISHITSUKA TETSUO (JP)
NOSE KOICHI (JP)
International Classes:
B22F7/08; B32B1/08; B32B15/01; C21D8/10; C22C30/00; C22C33/02; C22C38/00; C22C38/40; C22C38/44; C22C38/48; (IPC1-7): C21D8/10; B32B1/08; C22C38/00
Foreign References:
JPH04350149A1992-12-04
JPH07243007A1995-09-19
Other References:
See also references of EP 0834580A4
Download PDF: