Abstract:
A high-strength alloy and a preparation method therefor. The alloy contains the following elements by weight percent: 21-40% of Mn, 3.1-15% of Al, and 45-75.9% of Cu. The alloy is obtained by smelting and casting, and has good casting performance, high mechanical strength, and good toughness and corrosion resistance.
Inventors:
ZHANG FALIANG (CN)
LIU LIQIANG (CN)
GONG QING (CN)
LIU LIQIANG (CN)
GONG QING (CN)
Application Number:
PCT/CN2015/084824
Publication Date:
February 04, 2016
Filing Date:
July 22, 2015
Export Citation:
Assignee:
BYD CO LTD (CN)
International Classes:
C22C9/05; C22C30/02
Foreign References:
GB1382201A | 1975-01-29 | |||
CN1948531A | 2007-04-18 | |||
EP1995337A1 | 2008-11-26 | |||
GB1004159A | 1965-09-08 | |||
US3323913A | 1967-06-06 | |||
US5098654A | 1992-03-24 | |||
CN101012522A | 2007-08-08 |
Attorney, Agent or Firm:
TSINGYIHUA INTELLECTUAL PROPERTY LLC (CN)
北京清亦华知识产权代理事务所(普通合伙) (CN)
北京清亦华知识产权代理事务所(普通合伙) (CN)
Download PDF: