Abstract:
Provided is an asphalt mixture which is obtained by mixing an aggregate, an asphalt, a lubricative solidifying material and an alkaline additive, and which is characterized in that the lubricative solidifying material contains a saturated fatty acid having 6-30 carbon atoms at a ratio of 50-100% by weight. The present invention is able to provide an asphalt mixture which is capable of developing strength in a relatively short time after installation, and which is capable of providing a pavement that has high strength, excellent rut resistance and excellent bending properties.
Inventors:
MORIYASU HIROCHIKA (JP)
KOSHI KENTARO (JP)
HATAKEYAMA KEIGO (JP)
KOSHI KENTARO (JP)
HATAKEYAMA KEIGO (JP)
Application Number:
PCT/JP2017/024666
Publication Date:
February 01, 2018
Filing Date:
July 05, 2017
Export Citation:
Assignee:
MAEDA ROAD CONSTRUCTION CO LTD (JP)
International Classes:
E01C7/26; C08K3/00; C08K5/09; C08L95/00
Domestic Patent References:
WO2015107762A1 | 2015-07-23 |
Foreign References:
JP5939722B1 | 2016-06-22 | |||
JP2016124982A | 2016-07-11 | |||
JP2002332606A | 2002-11-22 | |||
JPH10310761A | 1998-11-24 | |||
JP2005528460A | 2005-09-22 | |||
JP2015050943A | 2015-03-19 | |||
JP2009221436A | 2009-10-01 | |||
US20070148356A1 | 2007-06-28 |
Other References:
See also references of EP 3492654A4
Attorney, Agent or Firm:
TOKOSHIE PATENT FIRM (JP)
Download PDF: