Abstract:
Provided is an austenitic heat resistant alloy containing, in mass%, 0.02-0.12% of C, at most 2.0% of Si, at most 3.0% of Mn, at most 0.030% of P, at most 0.015% of S, at least 20.0% and less than 28.0% of Cr, more than 35.0% and at most 55.0% of Ni, 0-20% of Co, 4.0-10.0% of W, 0.01-0.50% of Ti, 0.01-1.0% of Nb, less than 0.50% of Mo, less than 0.50% of Cu, at most 0.30% of Al, less than 0.10% of N, 0-0.05% of Mg, 0-0.05% of Ca, 0-0.50% of REM, 0-1.5% of V, 0-0.1% of B, 0-0.10% of Zr, 0-1.0% of Hf, 0-8.0% of Ta, and 0-8.0% of Re, with the remainder comprising Fe and inevitable impurities, wherein, in a cross section perpendicular to the longitudinal direction of the alloy, the shortest distance from the center to the outer surface portion is 40 mm or more, the austenite grain size number of the outer surface portion is -2.0 to 4.0, the amount of Cr present as a precipitate satisfies [CrPB/CrP S≤10.0], and [YSS/YSB≤1.5] and [TSS/TSB≤1.2] are satisfied at room temperature.

Inventors:
SEMBA HIROYUKI (JP)
OKADA HIROKAZU (JP)
YOSHIZAWA MITSURU (JP)
ONO TOSHIHIDE (JP)
Application Number:
PCT/JP2017/004824
Publication Date:
August 16, 2018
Filing Date:
February 09, 2017
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NIPPON STEEL & SUMITOMO METAL CORP (JP)
International Classes:
C22C19/05; C21D8/00; C22C38/00; C22C38/58; C22F1/10
Foreign References:
JP2011063838A2011-03-31
JP2004003000A2004-01-08
JP2016037664A2016-03-22
JPS61179833A1986-08-12
JPS61179834A1986-08-12
JPS61179835A1986-08-12
JPS61179836A1986-08-12
JP2004003000A2004-01-08
Other References:
See also references of EP 3581669A4
Attorney, Agent or Firm:
BRIGHTAS IP ATTORNEYS (JP)
Download PDF: