Abstract:
Provided are a composition serving as a binder having an excellent balance of suppressing deterioration of battery performance in a high-capacity electrode, high-temperature storage characteristics, and direct current resistance, and a slurry for a positive electrode, a positive electrode, and a secondary battery using said composition. Provided according to the present invention is a composition in which the component ratio of the component S180 is from 10% to 80% and the relaxation time of the component S180 is 500 μsec or longer when the free induction decay curve of the composition measured at 180°C by the solid echo method using pulse NMR is separated into three components: component S180, component M180, and component H180.

Inventors:
ISHIGAKI YUHEI (JP)
KANTO RYOSUKE (JP)
WATANABE JUN (JP)
Application Number:
PCT/JP2021/029651
Publication Date:
February 17, 2022
Filing Date:
August 11, 2021
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
DENKA COMPANY LTD (JP)
International Classes:
C08L51/06; C08F261/04; C08K3/04; C08L29/04; C08L33/02; C08L33/20; H01M4/13; H01M4/139; H01M4/505; H01M4/525; H01M4/62; H01M10/052; H01M10/054
Domestic Patent References:
WO2016024525A12016-02-18
WO2017154949A12017-09-14
WO2018230599A12018-12-20
WO2020162503A12020-08-13
WO2020162505A12020-08-13
WO2020209260A12020-10-15
WO2015053224A12015-04-16
WO2018230599A12018-12-20
Foreign References:
JP2000095823A2000-04-04
JPH06506252A1994-07-14
JP2010521798A2010-06-24
JP2001256980A2001-09-21
JP2013048043A2013-03-07
JP2004227974A2004-08-12
JP2013098123A2013-05-20
JP2013084351A2013-05-09
JPH06172452A1994-06-21
Other References:
See also references of EP 4198087A4
Attorney, Agent or Firm:
SK INTELLECTUAL PROPERTY LAW FIRM et al. (JP)
Download PDF: