CONDUIT REHABILITATION PIPE
Document Type and Number:
WIPO Patent Application WO/2014/061788
Kind Code:
A1
Abstract:
The purpose of the present invention is to not only ensure desired flat strength in a conduit rehabilitation pipe, but also to prevent tearing and wrinkling that may occur in a conduit rehabilitation pipe during drawing work. Provided is a conduit rehabilitation pipe characterized in comprising a lower-side soft resin layer (5d) constituting an inner layer of a straight pipe part (5b), an upper-side soft resin layer (5e) layered on the outer side of the lower-side soft resin layer (5d) and constituting an outer layer of the straight tube part, and a ridge part (5c) formed in a spiral shape on the outer surface of the upper-side soft resin layer (5e). The ridge part (5c) is composed of a core material (5g) made of hard resin wound in a spiral shape, and a core material coating part (5f) integrated with the upper-side soft resin layer (5e) in state enclosing the core material. The core material (5g) has a height that is 3.5% to 5% of the inside diameter of the straight pipe part (5b). The lower-side soft resin layer (5d) is formed by winding so as to include at least a single layer portion (5ds). The single layer portion (5ds) has a height that is 0.25% to 0.65% of the inside diameter of the straight pipe part (5b).

Inventors:
KANAO SHIGEKI (JP)
Application Number:
PCT/JP2013/078337
Publication Date:
April 24, 2014
Filing Date:
October 18, 2013
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
KANAFLEX CORP (JP)
International Classes:
B32B1/08; F16L1/00; F16L11/11; F16L55/18
Foreign References:
JP2012026524A2012-02-09
JP2012026516A2012-02-09
JP2006083608A2006-03-30
JP2005003189A2005-01-06
JPS60247544A1985-12-07
Attorney, Agent or Firm:
SAMEJIMA, Mutsumi et al. (JP)
Mutsumi Sameshima (JP)
Download PDF: