Abstract:
In a first cooling zone (21) on the upper side of a vertical section (20), an air-water ratio A1/R1 defined by a water amount R1 (L/min) and an air amount A1 (L/min) per one cooling spray nozzle is set to 10 or more, an impinging pressure of cooling water colliding with the surface of a slab (1) from the cooling spray nozzle is set to 12 gf/cm2 or more, a cooling intensity W1 × t1 defined by a cooling water density W1 (L/min/m2) and a passing time t1 (min) of the first cooling zone (21) is set to 350 or more, and a reheating time from the passage of the first cooling zone (21) to a bent portion (30) is set to 0.5 min or more.

Inventors:
TAKAYA SHIN (JP)
MURAKAMI TOSHIHIKO (JP)
Application Number:
PCT/JP2019/048269
Publication Date:
June 18, 2020
Filing Date:
December 10, 2019
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
NIPPON STEEL CORP (JP)
International Classes:
B22D11/124; B22D11/22
Foreign References:
JP2018099704A2018-06-28
JP2014050873A2014-03-20
JP2010253525A2010-11-11
JP2011131242A2011-07-07
JP2000237858A2000-09-05
Attorney, Agent or Firm:
TANAI Sumio et al. (JP)
Download PDF: