Abstract:
Provided is a high-strength steel sheet having: an element composition that includes, in mass%, C: 0.09-0.17% of C, Si: 0.6-1.7% of Si, 3.5% or less of Mn, 0.03% or less of P, 0.005% or less of S, 0.08% or less of Al, 0.006% or less of N, 0.05% or less of Ti, and 0.0002-0.0030% of B, the balance being Fe and unavoidable impurities; and a steel sheet structure that includes, in area percentage, less than 20% (including 0%) of a ferrite phase, 75% or more (including 100%) of a tempered martensite phase, 10% or less (including 0%) of a non-tempered martensite phase, and less than 5% (including 0%) of a residual austenite phase, the Vickers hardness of the tempered martensite phase being 280-340, and the tensile strength of the sheet being 950-1,120 MPa.
Inventors:
KOHSAKA NORIAKI (JP)
FUNAKAWA YOSHIMASA (JP)
SAKURAI MICHITAKA (JP)
SUZUKI YOSHIKAZU (JP)
FUNAKAWA YOSHIMASA (JP)
SAKURAI MICHITAKA (JP)
SUZUKI YOSHIKAZU (JP)
Application Number:
PCT/JP2016/000156
Publication Date:
September 09, 2016
Filing Date:
January 14, 2016
Export Citation:
Assignee:
JFE STEEL CORP (JP)
International Classes:
C22C38/00; C21D9/46; C22C38/14; C22C38/60; C23C2/06; C23C2/28; C23C2/40; C22C18/00
Foreign References:
JP2014029021A | 2014-02-13 | |||
JP2014196557A | 2014-10-16 | |||
JP2006183140A | 2006-07-13 | |||
JP2009209450A | 2009-09-17 | |||
JP2013227657A | 2013-11-07 | |||
JP2008038247A | 2008-02-21 | |||
JP2013032581A | 2013-02-14 | |||
JP2011225915A | 2011-11-10 |
Other References:
See also references of EP 3266894A4
Attorney, Agent or Firm:
KUMASAKA, Akira et al. (JP)
Akira Kumasaka (JP)
Akira Kumasaka (JP)
Download PDF:
Previous Patent: IMAGE PICKUP DEVICE
Next Patent: WATER TREATMENT APPARATUS AND OPERATION METHOD FOR WATER TREATMENT APPARATUS
Next Patent: WATER TREATMENT APPARATUS AND OPERATION METHOD FOR WATER TREATMENT APPARATUS