LOW-FRICTION COATING PRODUCTION METHOD AND SLIDING METHOD
Document Type and Number:
WIPO Patent Application WO/2016/121937
Kind Code:
A1
Abstract:
According to the present invention, a sliding surface 6, which is formed using a metal (SUJ2, palladium etc.) or an oxide ceramic (ZrO2), is made to slide, at a Hertz contact stress of 1.0 GPa or more in an atmospheric environment containing a hydrogen gas that includes a minute amount of an alcohol and water, against a surface 7 for sliding, said surface including a PLC film 9 which is a coating formed by means of an ionization deposition method while applying a low bias voltage. This makes it possible to form, on the sliding surface 6, a low-friction coating 5 that stably exhibits a significantly low friction coefficient in the order of 10-4 (less than 0.001).

Inventors:
KATO TAKAHISA (JP)
NOSAKA MASATAKA (JP)
TOHYAMA MAMORU (JP)
SUZUKI MASAHIRO (JP)
Application Number:
PCT/JP2016/052680
Publication Date:
August 04, 2016
Filing Date:
January 29, 2016
Export Citation:
Click for automatic bibliography generation   Help
Assignee:
JTEKT CORP (JP)
UNIV TOKYO (JP)
International Classes:
C23C16/26; C10M103/02; F16C19/00; F16C33/12; F16C33/24; F16C33/64
Foreign References:
JP2008522020A2008-06-26
JP2002097573A2002-04-02
JP2012246545A2012-12-13
JP2007099947A2007-04-19
JP2000144378A2000-05-26
JP2005145720A2005-06-09
JP2006291355A2006-10-26
Attorney, Agent or Firm:
UENO, HIDEKI (JP)
Ueno Hideki (JP)
Download PDF: